Set-recovery of heat treated maritime pine wood prior and after compression
Pine (Pinus pinaster) wood samples were subjected to a combined densification and heat treatment process. Samples were densified before and after heat treatment. The heat treatment was carried out inside an oven at 190ºC for 2 to 6 h and wood densification was performed in a hot press at around 48 b...