Synergistic helium and deuterium blistering in tungsten–tantalum composites

Tungsten–tantalum composites with 10 and 20 at.% Ta were prepared by ball milling W powder with Ta fibers and by consolidating the milled materials with spark plasma sintering. The composites were implanted at room temperature with He+ (30 keV with a fluence 5 1021 at/m2) and/or D+ (15 keV with a fl...

Full description

Bibliographic Details
Main Author: Dias, Marta (author)
Other Authors: Mateus, R. (author), Catarino, N. (author), Franco, N. (author), Nunes, D. (author), Correia, J.B. (author), Carvalho, Patricia Almeida (author), Hanada, K. (author), Sârbu, C. (author), Alves, E. (author)