Pine wood modification by heat treatment in air
Maritime pine (Pinus pinaster) wood has low dimensional stability and durability. Heat treatment was made in an oven using hot air during 2 to 24 h and at 170-200 ºC. A comparison was made against steam heat treatment. The equilibrium moisture content and the dimensional stability (ASE) in radial an...