Mode I interlaminar fracture of woven glass/epoxy multidirectional laminates
Mode I Double Cantilever Beam (DCB) tests were performed on woven glass/epoxy multidirectional laminates. Selected specimen stacking sequences with starter delaminations in theta/-theta and 0/theta interfaces were first evaluated with three-dimensional finite element (FE) models. During the DCB test...