Compressive strength of resin-modified glass ionomer restorative material: effect of P/L ratio and storage time

The aim of this study was to evaluate the compressive strength of resin-modified glass ionomer cement Fuji II LC and Vitremer, in powder/liquid ratios of 1:1, 1:2 and 1:3, at three periods (24 hours, 7 and 28 days) of storage in distilled water at 37ºC. For each material, P/L ratio and storage time,...