Surface properties of suberin

The surface energy of suberin was determined by four different methods, namely, (i) contact angle measurements, (ii) Wilhelmy plate measurements, (iii) maximum bubble pressure, and (iv) inverse gas chromatography (IGC). The first three methods gave a gammasub value in the range 40-50 mN m-1 at room...

Full description

Bibliographic Details
Main Author: Cordeiro, Nereida (author)
Other Authors: Aurenty, Patrice (author), Belgacem, Mohamed Naceur (author), Gandini, Alessandro (author), Neto, Carlos Pascoal (author)
Format: article
Language:eng
Published: 2021
Subjects:
Online Access:http://hdl.handle.net/10400.13/3373
Country:Portugal
Oai:oai:digituma.uma.pt:10400.13/3373
Description
Summary:The surface energy of suberin was determined by four different methods, namely, (i) contact angle measurements, (ii) Wilhelmy plate measurements, (iii) maximum bubble pressure, and (iv) inverse gas chromatography (IGC). The first three methods gave a gammasub value in the range 40-50 mN m-1 at room temperature. The major component of this value reflects the dispersive contribution. The IGC measurements showed a higher dispersive term, which is common with this method of characterization. The surface acid (A)/base (B) properties were also evaluated, and the results indicated that suberin has an acidic character.