Interlaminar Adhesive Strength of Nano-Reinforced Glass/Epoxy Laminates
Interlaminar fracture is significantly influenced by the adhesive strength of fiber=matrix interfaces. Critical strain energy release rate (GC) is the most common parameter used to quantify the interfacial strength. However, subcritical debonding can occur at lower mechanical loads than those requir...