Synergistic helium and deuterium blistering in tungsten–tantalum composites
Tungsten–tantalum composites with 10 and 20 at.% Ta were prepared by ball milling W powder with Ta fibers and by consolidating the milled materials with spark plasma sintering. The composites were implanted at room temperature with He+ (30 keV with a fluence 5 1021 at/m2) and/or D+ (15 keV with a fl...